Polymer Property : Tensile Strength, Ultimate = 0.861845 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.861845 - 64.8107 MPa

@Temperature -59.0 - 204 °C
125.000 - 9400.02 psi

@Temperature -74.2 - 399 °F
Average value: 9.14 MPa Grade Count:19
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..