Polymer Property : Tensile Strength, Ultimate = 0.870 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.870 MPa
126 psi
ASTM D 638
REXtac Rextac® RT 2215 Amorphous Polyalphaolefin (APAO)
Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance and flexibility, short open time, and good wettingApplications: Component of hot melt adhes..