Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.08 - 28.0 MPa
157 - 4060 psi
Average value: 9.90 MPa Grade Count:31
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini..
Tensile Strength, Ultimate 1.08 MPa
156 psi
JIS K6301
Stellarchem AB835EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..