Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.57 MPa | 228 psi | |
Momentive Performance Materials TSE392 One Component RTV Adhesive Sealant/Coating, Clear/White TSE392, TSE397 and TSE399 adhesive sealants/coatings are one component RTV’s that cure quickly by reacting with atmospheric moisture forming a soft dielectric silicone rubber. These materials i.. |
|||
Tensile Strength, Ultimate | 1.57 MPa | 228 psi | |
Momentive Performance Materials RTV6702 White Adhesive Sealant, General Purpose Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose adhesive sea.. |
|||
Tensile Strength, Ultimate | 1.57 MPa | 228 psi | |
Momentive Performance Materials RTV6703 Black Adhesive Sealant, General Purpose Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose adhesive sea.. |
|||
Tensile Strength, Ultimate | 1.57 MPa | 228 psi | |
Momentive Performance Materials RTV6708 Translucent Adhesive Sealant, General Purpose Paste One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose adhesive sea.. |