Polymer Property : Tensile Strength, Ultimate = 1014 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1014 MPa
147100 psi
Typical, Longitudinal Direction
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC)
Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martens..
Tensile Strength, Ultimate 1014 MPa

@Temperature 760 °C
147100 psi

@Temperature 1400 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Tensile Strength, Ultimate 1014 MPa
147100 psi
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Ultimate 1014 MPa
147100 psi
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Ultimate 1014 MPa
147100 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 40% Cold Rolled (UNS S30403)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..
Tensile Strength, Ultimate 1014 MPa
147100 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 40% Cold Rolled (UNS S30400)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..
Tensile Strength, Ultimate 1014 MPa
147100 psi
Typical Transverse
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA
Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, ..