Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1070 MPa
155000 psi
Pacific Sintered Materials FN-253-T(HT) 4600 Powdered Metal
High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals.
Tensile Strength, Ultimate 1070 MPa
155000 psi
PSM Industries Pacific Sintered Metals 4600 F-253-T(HT) Powdered Metal
High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-140HTInformation Provided by Pacific Sintered Metals, a division of PSM ..
Tensile Strength, Ultimate >= 1070 MPa
>= 155000 psi
PSM Industries PolyAlloys MIM-14-4PH Heat Treated Stainless Steel
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl..
Tensile Strength, Ultimate 1070 MPa
155000 psi
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 1070 MPa
155000 psi
In Core
Latrobe Lescalloy® 9310 VAC-ARC Premium Carburizing Steel
9310 VAC-ARC is a premium quality alloy carburizing steel produced by the vacuum consumable electrode process. It has a high hardenability, high core hardness and high fatigue strength, all of which..
Tensile Strength, Ultimate 1070 - 1310 MPa
155000 - 190000 psi
Materion Beryllium Nickel Strip - Alloy 360 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way)..
Tensile Strength, Ultimate 1070 - 1241 MPa
155000 - 180000 psi
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Tensile Strength, Ultimate 1070 MPa
155000 psi
Haynes 25 alloy, cold worked sheet, 10% cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 1070 - 1310 MPa
155000 - 190000 psi
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al..
Tensile Strength, Ultimate 1070 MPa
155000 psi
Special Metals Nitinol Superelastic Ni-Ti alloy
Special Metals Corporation is a producer of a series of "Nitinol" and other shape memory alloys used for a range of applications from precision engineering to medical technology.
Tensile Strength, Ultimate 1070 MPa
155000 psi
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..