Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 74.12 MPa | 10750 psi | ASTM D638 |
Nylene® Norpex® AX20MRFR , 20% Mineral Reinforced, Flame Retardant Polyphenylene Ether Description: Norpex® AX20MRFR is a 20% mineral reinforced, flame retardant PPE. AX20MRFR is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all opertin.. |