Polymer Property : Tensile Strength, Ultimate = 1090 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1090 MPa
158000 psi
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 1090 MPa
158000 psi
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1090 MPa
158000 psi
Haynes 214® alloy, sheet, 100 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1090 MPa
158000 psi
Typical
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Annealed
Features: TIMETAL 6-6-2 offers improved strength properties and greater depth hardenability compared with TIMETAL 6-4.Data provided by TIMET.