Polymer Property : Tensile Strength, Ultimate = 109800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 757.0 MPa
109800 psi
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, Solution Treated
Tensile strength (ultimate and yield), and elongation values reported here are typical for Cold Rolled Sheet, Solution Treated samples. Density and magnetic permeability are typical of annealed INCO..