Polymer Property : Tensile Strength, Ultimate = 113000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 770 - 780 MPa
112000 - 113000 psi
Kennametal Stellite Denertiaâ„¢ C14 Cobalt Chromium Dental Alloy
Denertia™ C14 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework. It conforms to the following International Standards: EN 1641 §..
Tensile Strength, Ultimate 580 - 780 MPa
84100 - 113000 psi
Minimum Guaranteed
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water ..
Tensile Strength, Ultimate 770 - 780 MPa
112000 - 113000 psi
Kennametal Stellite Denertiaâ„¢ C4 Cobalt Chromium Dental Alloy
Denertia™ C4 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.It conforms to the following International Standards: EN 1641 §4...
Tensile Strength, Ultimate 676 - 779 MPa
98000 - 113000 psi
Eagle Brass 519 Phosphor Bronzes 6%, Spring
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Ultimate 696 - 779 MPa
101000 - 113000 psi
Eagle Brass 64725 MAX251C, Spring
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Ultimate 570 - 780 MPa
82700 - 113000 psi
CLAL-MSX NICLAL 1300 H14 4/4 Hard Copper Alloy, Free Cutting Nickel-Silver
Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX