Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1135 MPa
164600 psi
Typical, Longitudinal Direction
Industeel CLC 1.2316 Prehardened (300HB) and Corrosion Resistant Mold Steel
Description: CLC 1.2316 is a 16%Cr 1% Mo with improved corrosion resistance properties, thanks to the chromium/molybdenum additions. The high cleanliness/homogeneity of the steel makes it specially ..
Tensile Strength, Ultimate 1135 MPa
164600 psi
Haynes 25 alloy, room temperature after 20% cold reduction, 1120°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..