Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.963 MPa | 1155 psi | post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4565 TBPB Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 7.963 MPa | 1155 psi | post cured- 2 hours at 177°C; ASTM D412 |