Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 12.9 MPa | 1870 psi | Original Properties; ASTM D412 Die C |
Freudenberg Simrit N431 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |
|||
Tensile Strength, Ultimate | 12.9 MPa | 1870 psi | Original Properties; ASTM D412 Die C |
Freudenberg Simrit N445 Nitrile Elastomer (NBR) General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings |
|||
Tensile Strength, Ultimate | 12.9 MPa | 1870 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8402 Polyolefin Elastomer Description: Engage® 8402 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8402 pr.. |