Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.75 MPa | 1270 psi | |
Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene Next Generation DOWLEX® IP-2580 resin is an improved processing linear low density polyethylene resin designed for excellent flow and stiffness with freezer grade impact properties. DOWLEX IP-2580 .. |
|||
Tensile Strength, Ultimate | 8.76 MPa | 1270 psi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Tensile Strength, Ultimate | 8.76 MPa | 1270 psi | After 7 days at 257°F (125°C); ASTM D573; ISO 188 |
Advanced Polymer Alloys Alcryn® 3055 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |