Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 7.61 - 8.99 MPa
1100 - 1300 psi
Arlon Flexible Silicon Insulation with Fiberglass Substrate (56493F031)
Side one - cured silicone rubber ,0.007 in. (0.18 mm) minimum: Substrate - Prime Coated 1564 Fiberglass, 0.017 in. (0.43 mm) nominal; Side two- cured silicone rubber, 0.007 in. (0.18 mm) minimum; 0...