Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 132.3 MPa | 19190 psi | ISO 527-1, 2 |
Polyplastics Duranex® HN7330 Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |