Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 133.4 MPa
19350 psi
ASTM D638
Plenco 51130 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51130 is an engineering grade UL flame rated glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in black only.Inform..
Tensile Strength, Ultimate 133.4 MPa
19350 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation.