Polymer Property : Tensile Strength, Ultimate = 1399 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1399 MPa
202900 psi
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr
Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h..
Tensile Strength, Ultimate 1399 MPa
202900 psi
Hardened 1800°F, Tempered 400°F
ATI Allegheny Ludlum 410 Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Ultimate 1399 MPa
202900 psi
Typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 204°C Temper
Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles..