Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 141 MPa
20500 psi
ASTM D638
Chevron Phillips Ryton® R-4 06 PPS (Polyphenylene Sulfide)  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Tensile Strength, Ultimate 141 MPa
20500 psi
ASTM D638
Adell BT-37 Nylon 6, 35% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 141 MPa
20500 psi
ASTM D638
Adell BT-17 Nylon 6, 35% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.