Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 925 - 990 MPa
134000 - 144000 psi
CLAL-MSX DECLAFOR® 1015 TH4 Wire quenched/Precipitation Heat Treated Copper Alloy
Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn..
Tensile Strength, Ultimate 689 - 993 MPa
99900 - 144000 psi
Typical, (Gauge, 0.028" -0.084")
AK Steel NITRONIC® 19-D Duplex Stainless Steel
AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}), good drawing and welding characteristi..
Tensile Strength, Ultimate 30.3 - 993 MPa
4400 - 144000 psi
Average value: 206 MPa Grade Count:30
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..