Polymer Property : Tensile Strength, Ultimate = 1442 psi
Polymer Property :
Tensile Strength, Ultimate =
1442 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
9.942
MPa
1442
psi
post cured- 8 hours at 177°C
Multibase SILASTIC® Q7-4750 Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase