Polymer Property : Tensile Strength, Ultimate = 15.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 15.1 MPa
2190 psi
Freudenberg Simrit V60WH Non-Black Compound
Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p..
Tensile Strength, Ultimate 15.1 MPa
2190 psi
DuPont Performance Polymers Kalrez® 6375 FFKM Perfluoroelastomer
Kalrez Spectrum 6375, designed specifically for the chemical process industry, combines new polymer technology with innovative patented curing technology. Compound 6375 is designed to give outstandi..