Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 105.9 MPa
15360 psi
ASTM D638
Plenco 51240 PET, Pellet, Injection Molded, Blue  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
Tensile Strength, Ultimate 105.9 MPa

@Temperature 150 °C
15360 psi

@Temperature 302 °F
ASTM D638
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..