Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 106 MPa | 15400 psi | ISO 527-1, 2 |
Polyplastics Duranex® 7307 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Tensile Strength, Ultimate | 106 - 133 MPa | 15400 - 19300 psi | Average value: 116 MPa Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |