Tensile Strength, Ultimate 1060 - 1210 MPa
154000 - 175000 psi
Materion Beryllium Copper Alloy 190 Strip; XHM (TM06) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate >= 1060 MPa
>= 154000 psi
Materion Brushform® 290 Beryllium Copper Alloy Strip; TM06 Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation after 1000 hrs @ 200°C: 78%Formability Ratio, 90° Bend, R..
Tensile Strength, Ultimate 1060 MPa
154000 psi
Misumi G-STAR Martensite Free-cutting Stainless Steel
Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation.
Tensile Strength, Ultimate 1060 MPa
154000 psi
Haynes 214® alloy, 40% cold reduction, 925°C for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1060 MPa
154000 psi
Haynes 25 alloy, room temperature after 20% cold reduction, 1175°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Ultimate 1060 MPa

@Temperature -196 °C
154000 psi

@Temperature -320 °F
Crucible Steel 20 Cb Plus Stainless Steel
Crucible 20 Cb Plus is a non-hardenable stabilized stainless steel with exceptional resistance to sulfuric, phosphoric, and nitric acid. This grade also has good resistance to stress corrosion crack..
Tensile Strength, Ultimate 1062 MPa

@Temperature -196 °C
154000 psi

@Temperature -321 °F
Longitudinal
Carpenter 20Cb-3® Stainless Steel
Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re..
Tensile Strength, Ultimate 1062 MPa

@Temperature -18.0 °C
154000 psi

@Temperature -0.400 °F
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Ultimate 1062 MPa

@Temperature 427 °C
154000 psi

@Temperature 801 °F
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Tensile Strength, Ultimate 1060 MPa
154000 psi
Industeel Superplast® Stainless Mold Steel
SUPERPLAST® Stainless is a specially designed steel for plastic mould bases providing improved performances compared to standard grades such as 1.2085. SUPERPLAST® Stainless offers improved machi..
Tensile Strength, Ultimate 1060 MPa

@Temperature 425 °C
154000 psi

@Temperature 797 °F
Haynes 242® alloy, hot rolled plate, annealed and aged