Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1089 MPa @Temperature -73.0 °C |
157900 psi @Temperature -99.4 °F |
|
Carpenter Custom 450® Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Ultimate | 1089 MPa | 157900 psi | |
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Ultimate | 1089 MPa @Temperature 538 °C |
157900 psi @Temperature 1000 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
Tensile Strength, Ultimate | 1089 MPa | 157900 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 40% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |