Polymer Property : Tensile Strength, Ultimate = 158.6 MPa
Polymer Property :
Tensile Strength, Ultimate =
158.6 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
158.6
MPa
23000
psi
ASTM D638
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).