Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 109 MPa
15800 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® AS-30CF/000 UV Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued
Description/Features:Carbon Fiber ReinforcedUV StabilizedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 109 MPa

@Temperature 427 °C
15800 psi

@Temperature 800 °F
Copper butt joint
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin..
Tensile Strength, Ultimate 109 MPa

@Temperature 427 °C
15800 psi

@Temperature 800 °F
Copper butt joint
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning ..
Tensile Strength, Ultimate 109 MPa
15800 psi
5 mm/min
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..