Tensile Strength, Ultimate >= 1590 MPa
>= 230000 psi
Kinetics MIM K3 Heat Treat
K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl..
Tensile Strength, Ultimate 1590 - 1600 MPa
230000 - 232000 psi
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 5.75 in RCS Billet Size High Strength Alloy Steel
LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi..
Tensile Strength, Ultimate 1590 MPa
231000 psi
Specialty Materials 5505 Boron Epoxy Prepreg Tape
Specialty Materials' 5505 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Exhibiting exceptional performance at temp..
Tensile Strength, Ultimate 1590 MPa
231000 psi
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi..
Tensile Strength, Ultimate 1590 MPa

@Temperature 316 °C
230000 psi

@Temperature 600 °F
Tempering Temperature-800°F
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..
Tensile Strength, Ultimate 1590 MPa
231000 psi
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction
The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f..
Tensile Strength, Ultimate 1590 MPa
230000 psi
Cold Worked 48%
Latrobe MP159® Alloy
MP159 is an alloy of the Multiphase family of alloys possessing the unique combination of ultra-high strength, ductility and corrosion resistance. Through work strengthening and aging, MP159 alloy ..