Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 1590 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1340 - 1590 MPa
194000 - 231000 psi
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Ultimate 1340 - 1590 MPa
194000 - 231000 psi
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Ultimate 1580 - 1590 MPa
229000 - 230000 psi
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 13.5 in RCS Billet Size High Strength Alloy Steel
LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi..
Tensile Strength, Ultimate 1310 - 1590 MPa
190000 - 231000 psi
Materion Beryllium Copper Alloy M25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17300)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Ultimate 1240 - 1590 MPa
180000 - 230000 psi
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the ..
Tensile Strength, Ultimate 1310 - 1590 MPa
190000 - 231000 psi
Materion Beryllium Copper Alloy 25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17200)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its ..
Copyright © lookpolymers.com All Rights Reserved