Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1619 MPa
234800 psi
Hardened 1900°F, Tempered 900°F
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Ultimate 1619 MPa
234800 psi
Typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 482°C Temper
Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai..