Polymer Property : Tensile Strength, Ultimate = 164.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 164.2 MPa
23820 psi
ASTM D638
Plenco 50030 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..