Tensile Strength, Ultimate 960 - 1140 MPa
139000 - 165000 psi
Materion Beryllium Copper Alloy 25 Wire; H (TD04) Temper; 1.3-2.0 mm Diameter (UNS C17200)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..
Tensile Strength, Ultimate 960 - 1140 MPa
139000 - 165000 psi
Materion Beryllium Copper Alloy M25 Wire; H (TD04) Temper; 1.3-2.0 mm Diameter (UNS C17300)
Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to..