Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1655 - 1862 MPa
240000 - 270100 psi
Materion Beryllium Nickel Strip - Alloy 360 MH10, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Tensile Strength, Ultimate 1655 MPa
240000 psi
HP Alloys Alloy 718, 30% Cold Worked, Aged
30% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..
Tensile Strength, Ultimate 1655 MPa
240000 psi
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950
AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala..
Tensile Strength, Ultimate 1655 MPa

@Temperature 426 °C
240000 psi

@Temperature 799 °F
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..