Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1517 - 1689 MPa
220000 - 245000 psi
Materion Beryllium Nickel Strip - Alloy 360 MH8, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..