Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1690 MPa | 245000 psi | Hardened 1900°F, Tempered 600°F |
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 1690 MPa | 245000 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 316°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Tensile Strength, Ultimate | 1690 MPa | 245000 psi | |
ATI Allvac® VascoMax® T-250 Specialty Steel, Heat Treatment: 816°C (1500°F) + Age Data provided by Allvac.Applications: Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts. |
|||
Tensile Strength, Ultimate | 1690 MPa | 245000 psi | Oil Quenched from 871°C; 427°C Temper Temperature |
Latrobe Staminal™ Shock Resisting Die Steel Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, .. |