Polymer Property : Tensile Strength, Ultimate = 17.06 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.06 MPa
2475 psi
Sylvin Technologies 8915-80 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 17.06 MPa
2475 psi
Sylvin Technologies 8940-85 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 17.06 MPa
2475 psi
Sylvin Technologies 9915-80 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 17.06 MPa
2475 psi
Sylvin Technologies 9940-85 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.