Polymer Property : Tensile Strength, Ultimate = 17.94 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.94 MPa
2602 psi
Abatron AboCast 8502-6/AboCure 8502-6 Colorless, Low-Exotherm Epoxy Casting Compound
AboCast 8502-6/AboCure 8502-6 is a flexible, colorless, low-exotherm epoxy casting compound for spherical masses up to 2000 grams. It is a 2-component structural and dielectric liquid system with lo..