Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1724 MPa | 250000 psi | |
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 1724 MPa @Temperature 316 °C |
250000 psi @Temperature 601 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Ultimate | 1724 MPa | 250000 psi | |
ATI Allvac® Vasco® 4340 Specialty Steel, Heat Treatment: 899°C (1650°F) Q+T Data provided by Allvac.Applications: Rocket motor cases, ordnance hardware, aircraft structural components, transmission gears, components, fasteners. |