Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 119 - 172 MPa
17300 - 25000 psi
Average value: 148 MPa Grade Count:18
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Tensile Strength, Ultimate 119 MPa
17300 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 441 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 119 MPa
17300 psi
ASTM D638
A. Schulman ComAlloy Voloy® 461 Glass Reinforced, PBT Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Ultimate 119 MPa
17300 psi
5mm/min; ISO 527
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G ..
Tensile Strength, Ultimate 119 MPa
17300 psi
ASTM D638
A. Schulman ComAlloy Comtuf® 463 Glass Reinforced, Impact Modified, PBT Alloy
Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..