Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1190 MPa
173000 psi
Haynes 556® alloy, 30% cold reduction
Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co..
Tensile Strength, Ultimate 1193 MPa
173000 psi
Haynes Hastelloy® G-30® alloy, 50% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Tensile Strength, Ultimate 1190 MPa

@Temperature 316 °C
173000 psi

@Temperature 600 °F
H900
Crucible Steel 15-5 Precipitation Hardening Stainless Steel
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V..
Tensile Strength, Ultimate 1190 MPa

@Temperature 316 °C
173000 psi

@Temperature 600 °F
H900
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a..
Tensile Strength, Ultimate 1190 MPa

@Temperature 316 °C
173000 psi

@Temperature 600 °F
H900
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. ..
Tensile Strength, Ultimate 1193 MPa
173000 psi
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Ultimate 1193 MPa
173000 psi
20% Cold Work
AK Steel NITRONIC® 30 Austenitic Stainless Steel
AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi..
Tensile Strength, Ultimate 1190 MPa
173000 psi
Long.
ATI Wah Chang 425™ Titanium Alloy, Solution Treated Annealed Bar 0.5 - 1.23 in. dia
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..