Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 12.380 MPa | 1795.6 psi | After 7 days at 70°C; ASTM D412 ISO 37 |
Advanced Polymer Alloys DuraGrip™ 6170 BK Melt Processable Elastomer DuraGrip™ 6170BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6170BK has an excellent
soft touch feel a.. |