Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1840 MPa | 267000 psi | |
Latrobe Marvac 250 VIM-VAR ; 5 in. High Strength Maraging Steel MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |
|||
Tensile Strength, Ultimate | 1840 MPa | 267000 psi | 524°C Temper Temperature |
Latrobe CSS-42L™ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness .. |