Polymer Property : Tensile Strength, Ultimate = 18500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 128 - 182 MPa
18500 - 26400 psi
Average value: 151 MPa Grade Count:5
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v..
Tensile Strength, Ultimate 127 MPa
18500 psi
DIN 53455; ASTM D638
Kolon KOPA® KN133G33HIBL G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 127 MPa
18500 psi
DIN 53455; ASTM D638
Kolon KOPA® KN333HB640BL Multi Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Tensile Strength, Ultimate 127 MPa
18500 psi
DIN 53455; ASTM D638
Kolon KOPET® KP133G30 FR-PET Resin
KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of..
Tensile Strength, Ultimate 127 MPa
18500 psi
Shinil Chemical SHINFLAME PBT GF Flame Retardant Polymer Lamp Housing
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod..
Tensile Strength, Ultimate 127 MPa
18500 psi
5mm/min; ASTM D638
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.