Polymer Property : Tensile Strength, Ultimate = 185900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1282 MPa
185900 psi
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction + Aged 538°C (1000°F)/4hr/AC
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Ultimate 1282 MPa

@Temperature 371 °C
185900 psi

@Temperature 700 °F
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Ultimate 1282 MPa
185900 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..
Tensile Strength, Ultimate 1282 MPa
185900 psi
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400)
This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to ..