Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 19.2 MPa | 2790 psi | Cured |
KKPC KOSYN KBR 01L Polybutadiene Rubber (High cis BR) Polybutadiene Rubber (High cis BR)Characteristics: Polybutadiene Rubber (BR), which has three kinds of bond structure of cis-1,4, trans-1,4, vinyl, is simple polymer made from 1,3-butadiene by solut.. |
|||
Tensile Strength, Ultimate | 19.2 MPa | 2780 psi | ASTM D412-80 |
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Peroxide Cured Carbon Black Filled Compound Carbon black compound with 100 parts Hypalon; 40 parts carbon black; 20 parts magnesia; and 5.8 parts Varox® DBPH-50. Physical property data below (except mooney viscosity) are for vulcanizate. Ma.. |