Polymer Property : Tensile Strength, Ultimate = 1900 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1900 MPa
276000 psi
204°C Temper Temperature
Latrobe Lescalloy® 4340 VAC-ARC ; 3.5" round High Strength Alloy Steel
LESCALLOY 4340 VAC-ARC steel is a low alloy, nickel-chromium-molybdenum steel capable of being heat treated to high strength levels. The alloy has a good combination of ductility, toughness and str..
Tensile Strength, Ultimate 1900 MPa
276000 psi
Cytec Thornel® P-55S 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the interla..
Tensile Strength, Ultimate 1900 MPa
276000 psi
Cytec Thornel® P-75S 2K Carbon Fiber, Pitch Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus strands made from a pitch precursor. The fiber surface has been treated to increase the i..
Tensile Strength, Ultimate 1900 MPa
275000 psi
hardness of 52 HRC
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel
Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic..
Tensile Strength, Ultimate 1900 MPa
276000 psi
AIM 80Au/20Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.
Tensile Strength, Ultimate 1900 MPa

@Temperature 23.0 °C
276000 psi

@Temperature 73.4 °F
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..