Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1334 MPa | 193500 psi | |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, 2 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness Tensile strength (ultimate and yield), shear strength, and elongation values reported here are typical for Cold Rolled Sheet, 2 Part Heat Treatment, 0.040 inch (1.02 mm) Thickness samples. Density a.. |
|||
Tensile Strength, Ultimate | 1334 MPa | 193500 psi | |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Hot Finished Flat, 2 Part Heat Treatment, 1.250 inch (31.8 mm) Thickness Tensile strength (ultimate and yield), shear strength, compressive strength, reduction of area, and elongation values reported here are typical for Hot Finished Flat, 2 Part Heat Treatment, 1.250 in.. |