Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1964 MPa | 284900 psi | |
ATI Allvac® Nickelvac® 43-40 UNS G43400, UNS H43400 Specialty Steel Uses: Automotive applications, structural components, gears, rods, heat-treatable shafts.Property values are for samples in the metallurgical condition: 1550°F quench + 1000°F temper.Information p.. |
|||
Tensile Strength, Ultimate | 1964 MPa | 284900 psi | |
ATI Allvac® Vasco® 440 C UNS S44004 Specialty Steel Uses: Bearing applications including ball bearing assemblies, valve seats and stems, check valve components, bushings.Property values are for samples in the metallurgical condition: 1525FC Quench + .. |