Polymer Property : Tensile Strength, Ultimate = 199600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1376 - 1757 MPa
199600 - 254800 psi
Latrobe Magnadie - RF Modified Premium H-13 Hot Work Die Steel
Magnadie-RF is a premium quality 5% chromium hot work die steel. The chemistry of Magnadie-RF steel is a modification of the premium quality H-13 chemistry. Magnadie-RF steel is designed for incre..